Inconel 660 (UNS S66286 / SUH660 / GH2132 /W.Nr. 1.4980) waa qalab aad u adag oo ku salaysan roobka oo leh awood heer sare ah iyo iska caabin oksaydh ilaa 704°C (1300°F). Womic Steel waxay ku siisaa Inconel 660 qaabab badan oo wax soo saar ah oo ay ku jiraan tuubo aan kala go 'lahayn, tuubo alxan, bir bir ah, saxan bir ah, gariirad bir ah, xariijin, flanges, rakibaado, foornooyin, silig, iyo dhejiyeyaal loogu talagalay codsiyada hawada sare, marawaxadaha gaaska, baabuurta, nukliyeerka, iyo batroolka.


Faahfaahinta Badeecada

Calaamadaha Alaabta

Waa maxay Inconel 660?

Inconel 660 waa bir ah oo ay ku badan tahay nickel-chromium oo ay xoojisay roobka marxaladda γ' [Ni₃(Al,Ti)] inta lagu jiro daaweynta kulaylka gabowga. Daawadu waxay ka kooban tahay qiyaastii 24-27% nickel, 13.5-16% chromium, iyo ku darista titanium (1.9-2.35%), aluminium (0.10-0.35%), molybdenum (1.0-1.5%), iyo vanadium (0.10-0.50%). Waxaa loogu talagalay codsiyada u baahan xoog sare ilaa 700°C oo leh iska caabin wanaagsan oo oksaydh iyo daxal.

Darajada 660 waxaa loo yaqaanaa:

●Xoogga heerkulka sareilaa 704°C (1300°F)

●Iska caabin aad u fiican oo jabitaan-jab ahheerkul sare

●Roobab adagiyada oo loo marayo daaweynta kulaylka gabowga caadiga ah

●Iska caabin oksaydh wanaagsanilaa 815°C

●Iska caabbinta nasashada walbahaarkaheerkul sare

●Ma-magnet ahaynguryaha

●Wax-soo-saarka wanaagsaniyo mashiin-sameyn

Halabuurka Kiimikada

Walax UNS S66286 (ASTM) SUH660 (JIS) GH2132 (GB) Doorka
Nikkel (Ni) 24.0 – 27.0 24.0 – 27.0 24.0 – 27.0 Xasilinta Austenite, iska caabinta daxalka
Chromium (Cr) 13.5 – 16.0 13.5 – 16.0 13.5 – 16.0 Iska caabbinta oksaydhka, carbide hore
Molybdenum (Mo) 1.0 – 1.5 1.0 – 1.5 1.0 – 1.5 Xoojinta xalka adag
Titanium (Ti) 1.90 – 2.35 1.90 – 2.35 1.90 – 2.35 Roobabka γ, adkaanta da'da
Aluminium (Al) 0.10 – 0.35 ≤ 0.35 ≤ 0.35 Roobabka γ'
Vanadium (V) 0.10 – 0.50 0.10 – 0.50 0.10 – 0.50 Hagaajinta hadhuudhka, carbide hore
Boron (B) 0.003 – 0.010 0.001 – 0.010 0.001 – 0.010 Xoojinta xadka miraha
Cobalt (Co) ≤ 1.00 ≤ 1.00 ≤ 1.00 Walax haraaga ah
Bir (Fe) Dheelitirnaan Dheelitirnaan Dheelitirnaan Qaybta salka ah
Kaarboon (C) ≤ 0.08 ≤ 0.08 ≤ 0.08 Carbide hore
Silikoon (Si) ≤ 1.00 ≤ 1.00 ≤ 1.00 Deoksaydheeyaha
Manganese (Mn) ≤ 2.00 ≤ 2.00 ≤ 2.00 Deoksaydheeyaha
Fosfooraska (P) ≤ 0.025 ≤ 0.040 ≤ 0.030 Nadaafad
Sulfur (S) ≤ 0.025 ≤ 0.030 ≤ 0.020 Nadaafad

Sifooyinka Farsamada

Xaalad Xanuunsan (Xalka La Daweeyay)

Hantida ASTM A453 Fasalka 660 Qiimaha
Xoogga Tijaabada ≤ 724 MPa (105 ksi)  
Xoogga Wax Soo Saarka (0.2% Ka Dhigista) -  
Kordhinta ≥ 25%  
Adkaanta ≤ 91 HRB

Xaalad Da' ah (Roob adag)

Hantida ASTM A453 Fasalka 660 Caadiga ah ee la gaaray
Xoogga Tijaabada ≥ 965 MPa (140 ksi) 1,000 – 1,100 MPa
Xoogga Wax Soo Saarka (0.2% Ka Dhigista) ≥ 655 MPa (95 ksi) 700 – 800 MPa
Kordhinta ≥ 15% 18 - 25%
Adkaanta 24 - 35 HRC 28 - 32 HRC
Xoogga Firfircoon (650°C, 100h) ≈ 240 MPa  
Xoog Qodxan (700°C, 100h) ≈ 210 MPa

Sifooyinka Jirka

Hantida Qiimaha
Cufnaanta 7.95 g/cm³
Kala duwanaanshaha Dhalmada 1371 – 1427°C
Qaboojinta Kulaylka 15.0 W/m·K heerkul ah 150°C
Isugeynta Ballaarinta Kulaylka 16.8 × 10⁻⁶/°C (20-100°C)
Modulus Laablaaban 201 GPA
Joogitaanka birlabeed Ma-magnet ahayn

Faa'iidooyinka Muhiimka ah ee Inconel 660

Xoogga Heerkulka Sare– Inconel 660 waxay ilaalisaa xoog sare oo jiidis ah, daal, iyo gariir-jeexitaan ah ilaa 704°C. Habka xoojinta roobka γ' wuxuu bixiyaa xoog heer sare ah marka loo eego biraha aan lahayn austenitic ee caadiga ah. Daloolada waxaa badanaa loo isticmaalaa boolal turbine ah iyo dhejiyeyaasha halkaas oo iska caabbinta nasashada ay muhiim tahay.

Iska caabin aad u fiican oo ku saabsan qulqulka-jabka– Daawadu waxay muujisaa iska caabin aad u fiican heerkulka sare. Nolosha gariirka-jabitaanka ee 650°C waxay ka badan tahay 1,000 saacadood iyadoo cadaadis dhexdhexaad ah uu jiro, taasoo ka dhigaysa agab lagu kalsoonaan karo oo loogu talagalay codsiyada adeegga heerkulka sare ee muddada dheer.

Iska caabinta Oksijiinta iyo Daxalka oo Wanaagsan– Iyada oo leh 13.5-16% chromium, Inconel 660 waxay bixisaa iska caabin wanaagsan oo ku saabsan oksaydhaynta, cabbirka, iyo daxalka heerkulka sare. Daxalkani si fiican ayuu ugu shaqeeyaa jawi oksaydhaynta ilaa 815°C wuxuuna iska caabiyaa warbaahinta kala duwan ee daxalka.

Roobab adag– Inconel 660 waxaa lagu adkeyn karaa roobabka iyadoo la adeegsanayo daaweynta kulaylka gabowga. Wareegga gabowga ee caadiga ah (675-705°C, 12-16 saacadood) wuxuu horumariyaa sifooyin farsamo oo ugu fiican wuxuuna bixiyaa iska caabin nasasho walaac oo aad u fiican, taas oo muhiim u ah codsiyada bolting.

Iska caabinta Daalka Wanaagsan– Daawadu waxay bixisaa iska caabin aad u fiican oo ku wajahan daalka iyo daalka kulaylka, taasoo ka dhigaysa mid ku habboon qaybaha ku xiran rarista wareegga heerkulka sare. Tani waxay si gaar ah muhiim ugu tahay codsiyada marawaxadaha iyo qaybaha matoorka.

Shaqo-karti iyo Machinability Aad u Fiican– Inconel 660 wuxuu leeyahay mashiin ka wanaagsan kuwa kale ee superalloys. Si fudud ayaa loo farsameyn karaa, si kulul ayaa loo shaqayn karaa, qabowna waa loo shaqayn karaa. Daloolada waxaa lagu alxan karaa iyadoo la isticmaalayo TIG, MIG, iyo alxanka iska caabbinta iyadoo la adeegsanayo biraha buuxinta ee ku habboon.

Faa'iidooyinka Muhiimka ah ee Inconel 660

Xoogga Heerkulka Sare– Inconel 660 waxay ilaalisaa xoog sare oo jiidis ah, daal, iyo gariir-jeexitaan ah ilaa 704°C. Habka xoojinta roobka γ' wuxuu bixiyaa xoog heer sare ah marka loo eego biraha aan lahayn austenitic ee caadiga ah. Daloolada waxaa badanaa loo isticmaalaa boolal turbine ah iyo dhejiyeyaasha halkaas oo iska caabbinta nasashada ay muhiim tahay.

Iska caabin aad u fiican oo ku saabsan qulqulka-jabka– Daawadu waxay muujisaa iska caabin aad u fiican heerkulka sare. Nolosha gariirka-jabitaanka ee 650°C waxay ka badan tahay 1,000 saacadood iyadoo cadaadis dhexdhexaad ah uu jiro, taasoo ka dhigaysa agab lagu kalsoonaan karo oo loogu talagalay codsiyada adeegga heerkulka sare ee muddada dheer.

Iska caabinta Oksijiinta iyo Daxalka oo Wanaagsan– Iyada oo leh 13.5-16% chromium, Inconel 660 waxay bixisaa iska caabin wanaagsan oo ku saabsan oksaydhaynta, cabbirka, iyo daxalka heerkulka sare. Daxalkani si fiican ayuu ugu shaqeeyaa jawi oksaydhaynta ilaa 815°C wuxuuna iska caabiyaa warbaahinta kala duwan ee daxalka.

Roobab adag– Inconel 660 waxaa lagu adkeyn karaa roobabka iyadoo la adeegsanayo daaweynta kulaylka gabowga. Wareegga gabowga ee caadiga ah (675-705°C, 12-16 saacadood) wuxuu horumariyaa sifooyin farsamo oo ugu fiican wuxuuna bixiyaa iska caabin nasasho walaac oo aad u fiican, taas oo muhiim u ah codsiyada bolting.

Iska caabinta Daalka Wanaagsan– Daawadu waxay bixisaa iska caabin aad u fiican oo ku wajahan daalka iyo daalka kulaylka, taasoo ka dhigaysa mid ku habboon qaybaha ku xiran rarista wareegga heerkulka sare. Tani waxay si gaar ah muhiim ugu tahay codsiyada marawaxadaha iyo qaybaha matoorka.

Shaqo-karti iyo Machinability Aad u Fiican– Inconel 660 wuxuu leeyahay mashiin ka wanaagsan kuwa kale ee superalloys. Si fudud ayaa loo farsameyn karaa, si kulul ayaa loo shaqayn karaa, qabowna waa loo shaqayn karaa. Daloolada waxaa lagu alxan karaa iyadoo la isticmaalayo TIG, MIG, iyo alxanka iska caabbinta iyadoo la adeegsanayo biraha buuxinta ee ku habboon.

Daaweynta Kulaylka ee Inconel 660

Inconel 660 waa daawaha roobka-adag ee u baahan daaweyn kuleyl gaar ah si loo gaaro sifooyin farsamo oo ugu fiican:

Xalka Qaboojinta (Xaaladda A):

●Heerkulka:980 – 1010°C (1800 – 1850°F)

●Waqtiga Qoynta:1 saac

●Qaboojinta:Qaboojinta degdega ah (damida saliidda ama biyaha)

●Ujeeddo:Kala dir dhammaan daadashada, gaar austenite hal-marxal ah

●Natiijo:Xaalad jilicsan, shaqeyn karta, diyaar u ah sameynta iyo farsamaynta

Adkaynta Roobabka (Gabawga - Xaaladda B):

●Heerkulka:675 – 705°C (1250 – 1300°F)

●Waqtiga Qoynta:12 - 16 saacadood

●Qaboojinta:Qabow hawo leh

●Ujeeddo:Foomka Ni₃(Al,Ti) γ' wuxuu soo dedejiyaa xoojinta

●Natiijo:Xoogga ugu badan iyo iska caabinta gurguurta

Gabow Laba Jibaaran (Beddel):

● Marxaladda Koowaad: 705°C muddo 16 saacadood ah, foornadana way qaboojisaa ilaa 620°C

● Marxaladda Labaad: 620°C muddo 16 saacadood ah, hawo qabow

●Ujeeddo:Hagaaji iska caabbinta nasashada walbahaarka ee codsiyada bolting

Foomamka Badeecadaha ee laga heli karo Womic Steel

Tuubo aan kala go 'lahayn iyo Tuubo aan kala go' lahayn

●Dhexroorka Dibadda:6mm – 200mm

●Dhumucda Darbiga:1mm – 25mm

●Dhererka:Ilaa 12m

●Heerarka:ASTM B639, ASTM B983, AMS 5731, AMS 5732, AMS 5737, AMS 5895

●Codsiyada:Tuubooyinka habka heerkulka sare leh, tuubooyinka isweydaarsiga kulaylka, khadadka qalabka, tuubooyinka hawada sare

●Erayada muhiimka ah:Tuubo aan kala go 'lahayn oo Inconel 660 ah, tuubo Fasalka 660 ah, tuubo UNS S66286 ah, tuubo SUH660 ah, tuubo 1.4980 ah oo aan kala go 'lahayn

Birta Birta ah (Goobo, Labajibbaaran, Fidsan, Hex)

●Dhexroorka:6mm – 300mm

●Dusha sare:Kulul la duubay, dhalaalaya (qabow la sawiray), Dhul, La rogay

●Heerarka:ASTM A453, ASTM B639, AMS 5731, AMS 5732, AMS 5734, AMS 5737

●Codsiyada:Boolal marawaxadaha, dhejisyada, burooyinka, ulaha, jirridda waalka, kaydka mishiinka

●Erayada muhiimka ah:Inconel 660 wareeg ah, Fasalka 660, usha SUH660, ASTM A453 Fasalka 660, qalabka lagu xiro heerkulka sare

Saxanka Birta ah iyo Xaashida

●Dhumucda:1mm – 100mm

●Ballaca:Ilaa 2000mm

●Heerarka:AMS 5525, AMS 5858

●Codsiyada:Qaybaha xididdada cadaadiska, qaybaha dhismaha, meelaha banaan ee flange

●Erayada muhiimka ah:Saxanka Inconel 660, warqadda fasalka 660, saxanka daawaha, saxanka heerkulka sare leh

Birta gariiradda iyo xarigga

●Dhumucda:0.5mm – 4.0mm

●Ballaca:10mm – 1000mm

●Heerarka:AMS 5525

●Codsiyada:Qaybaha la sameeyay, bullaacadaha, shaambadaynta

●Erayada muhiimka ah:Inconel 660 gariirad, xariijin, xariijin heerkul sare leh

Flanges & Qalabka lagu rakibay

●Noocyada:Luqunta Alxanka, Simbiriirixan, Indho la'aan, Alxanka godka, dunta lagu dhejiyay

●Cabbirrada:1/2" – 24"

●Qiimaynta Cadaadiska:Fasalka 150 - Fasalka 2500

●Heerarka:ASTM A453, ASME B16.5

●Erayada muhiimka ah:Flanges-ka Inconel 660, Qalabka Heerka 660

Farshaxanno

●Noocyada:Giraangiraha, saxannada, ulaha, jirrooyinka waalka, joomatari gaar ah

●Miisaanka:Ilaa 3,000kg gabalkiiba

●Heerarka:ASTM A453, AMS 5731

●Erayada muhiimka ah:Inconel 660 oo ah farshaxan, faraanti been abuur ah, oo ah farshaxan qayb ka ah mashiinka turbine-ka

Xidhayaasha (Buulto, Laws, iyo Xargo)

●Noocyada:Boolal Hex ah, boolal madaxa godka ah, boolal bir ah, Ulo dunaysan, Laws, Makiinadaha dhaqda

●Cabbirrada:M2 – M100, 1/4" – 4"

●Heerarka:ASTM A453 Fasalka 660, ASTM B637

●Codsiyada:Boolal turbine ah, isku xirka flange-ka heerkulka sare leh, qalabka dhismaha

●Erayada muhiimka ah:Boolal Inconel 660, Boolal bir ah oo heer sare ah oo loogu talagalay fasalka 660, qalab lagu xiro heerkulka sare, boorsooyin turbine ah

Qalliinka Fasalka 660

●Noocyada:Waalalka kubbadda, Waalalka albaabka, Waalalka adduunka, Waalalka hubi

●Cabbirrada:1/2" – 12"

●Qiimaynta Cadaadiska:Fasalka 150 - Fasalka 2500

●Kala Duwanaanshaha Heerkulka:-196°C ilaa +704°C

●Heerarka Naqshadeynta:API 608, API 6D, ASME B16.34

●Dhaqdhaqaaq:Gacan, Pneumatic, Koronto

●Codsiyada:Kala-goynta habka heerkulka sare, khadadka uumiga marawaxadaha, xakamaynta marawaxadaha gaaska

Fasalka 660 iyo Inconel 718: Isbarbardhigga

Inconel 660 iyo Inconel 718 labaduba waa alloys aad u adag oo roobka adkeeya, laakiin waxay leeyihiin kala duwanaansho kala duwan:

Inconel 660 - Daawaha Heerkulka Sare ee Ku Salaysan Birta

●Qaybta Aasaaska ah:Birta (dheelitirka) oo leh 24-27% Ni

●Marxaladda Xoojinta:γ' (Ni₃(Al,Ti))

●Xoogga Garaacista (da'da):≥ 965 MPa

●Awoodda heerkulka:Ilaa 704°C

●Codsiyada Muhiimka ah:Boolal marawaxadaha, dhejisyada, boolal, qaybaha matoorka jet-ka

●Qiimaha:Ka dhaqaale badan 718 oo ku salaysan nikkel

●Inconel 718 - Superalloy ku salaysan Nickel

●Qaybta Aasaaska ah:Nikkel (50-55%) oo leh 18-20% Fe

●Marxaladaha Xoojinta:γ' (Ni₃Al) + γ'' (Ni₃Nb)

●Xoogga Garaacista (da'da):≥ 1,240 MPa

●Awoodda heerkulka:Ilaa 700°C

●Codsiyada Muhiimka ah:Saxannada marawaxadaha, matoorada gantaalada, saliidda iyo gaaska HPHT

Goorta la dooranayo Fasalka 660:Codsiyada u baahan boolal heerkul sare leh iyo xidhitaan, qaybaha matoorka jet-ka, boolal turbine ah, iyo baabuur waxqabad sare leh halkaas oo kharashku yahay qodob iyo xoog sare ilaa 700°C ayaa loo baahan yahay.

Goorta la dooranayo Inconel 718:Codsiyada u baahan xoog heerkul sare oo ugu badan, adkaanta jabka, iyo iska caabbinta gurguurta heerkulka ilaa 700°C halkaas oo kharashku ka yar yahay walaac.

Heerarka & Tilmaamaha

Heerka Caadiga ah Sharaxaad
Magacaabista Qaramada Midoobay S66286
Lambarka Werkstoff 1.4980
AISI/SAE 660
ASTM A453 Qeexitaanka caadiga ah ee bolting heerkulka sare
ASTM B639 Baar/ul daawaha heerkulka sare leh
AMS 5525 Saxan/xaashi/xariiq
AMS 5731 Baar, silig, foornooyin
AMS 5732 Baar, silig, foornooyin
AMS 5734 Baar, silig, foornooyin
AMS 5737 Tuubo iyo tuubo
AMS 5895 Baar, silig, foornooyin
JIS SUH660
GB/T GH2132
Yurub 1.4980 / X6NiCrTiMoV25-15-2
ISO X6NiCrTiMoV25-15-2

Codsiyada Inconel 660

Hawada Sare– Inconel 660 waxaa si ballaaran loogu isticmaalaa qaybaha matoorka jet iyo gaaska oo ay ku jiraan boolal turbine ah, saxannada kombaresarada, khaanadaha turbine-ka, qaybaha gubashada, rogaal celiyaasha riixitaanka, iyo qalabka rakibaadda matoorka. Isku-darka xoogga heerkulka sare, iska caabbinta daalka, iyo iska caabbinta oksaydhka ayaa ka dhigaysa mid ku habboon codsiyada hawada sare ee muhiimka ah. Daloolku waa agab caadi ah oo loogu talagalay boolal matoorka jet-ka iyo dhejiyeyaasha ku shaqeeya heerkulka ilaa 700°C.

Soo saarista Korontada Gaaska ee Turbine-ka– Daloolada waxaa loo isticmaalaa boolal turbine ah, boolal, iyo qalab lagu xidho turbines-ka gaaska warshadaha, turbines-ka uumiga, iyo warshadaha korontada ee isku dhafan. Iska caabbintiisa nasashada cadaadiska heerkulka sare waxay hubisaa isku xirnaanta la isku halleyn karo iyada oo loo marayo cimri dheer.

Gawaarida– Inconel 660 waxaa loo isticmaalaa guryaha turbocharger-ka, qalabka qiiqa, qaybaha matoorka naaftada, iyo qalabka wax lagu xiro ee baabuurta ee waxqabadka sare leh. Awooddeeda ay u leedahay inay u adkaysato heerkulka gaaska qiiqa iyo wareegga kulaylka ayaa ka dhigaysa mid ku habboon matoorada casriga ah ee waxqabadka sare leh iyo kuwa turbocharged-ka leh.

Awoodda Nukliyeerka– Daloolada waxaa loo isticmaalaa qaybaha fal-galiyaha nukliyeerka, gudaha gudaha, farsamooyinka xakamaynta usha, iyo qalabka heerkulka sare leh ee u baahan isku halaynta muddada dheer iyo iska caabbinta shucaaca neutron-ka.

Habaynta Kiimikada Batroolka– Inconel 660 waxaa loo isticmaalaa fal-galayaasha kiimikada heerkulka sare leh, tuubooyinka dib-u-hagaajinta, qaybaha foornada, iyo tuubooyinka habka u baahan xoog iyo iska caabin oksaydh heerkul sare.

Bolting Heerkulka Sare– Darajada 660 waa agabka caadiga ah ee loogu talagalay codsiyada bolting heerkulka sare. Boolal iyo birlabyo ASTM A453 Fasalka 660 si weyn ayaa loogu cayimay flanges-ka xididdada cadaadiska, dahaarka marawaxadaha, iyo isku xirka tuubooyinka heerkulka sare leh ee u baahan iska caabinta gurguurta iyo nasashada walbahaarka.

Su'aalaha Badiya La Weydiiyo

S: Waa maxay Inconel 660?

A: Inconel 660 (UNS S66286 / SUH660 / GH2132) waa bir-adayg sare oo roob-adayg ah oo leh xoog heerkul sare oo heer sare ah ilaa 704°C. Waxaa xoojiya roobka γ' iyada oo loo marayo daaweynta kulaylka gaboobaya waxaana si weyn loogu isticmaalaa boolal turbine ah, dhejisyo, iyo qaybaha matoorka jet-ka.

S: Waa maxay faraqa u dhexeeya Darajada 660 iyo Inconel 718?

A: Inconel 660 wuxuu ku salaysan yahay birta (oo leh 24-27% Ni, dheelitirka Fe) oo leh xoog jiidis ≥ 965 MPa, halka Inconel 718 uu ku salaysan yahay nikkel (50-55% Ni) oo leh xoog jiidis ≥ 1,240 MPa. Heerka 660 waa mid dhaqaale ahaan ka dhaqaale badan oo si weyn loogu isticmaalo bolting; Inconel 718 waxaa loo isticmaalaa codsiyada xoogga ugu badan.

S: Waa maxay heerkulka ugu sarreeya ee adeegga ee Inconel 660?

A: Inconel 660 waxaa loo qiimeeyay adeeg joogto ah ilaa 704°C (1300°F). Iska caabbinta oksaydhka, safarro gaaban oo ilaa 815°C (1500°F) ah ayaa suurtagal ah. Xoogga gurguurta ayaa si weyn hoos ugu dhacaya 700°C.

S: Inconel 660 ma si fudud loo alxan karaa?

J: Haa, Inconel 660 waxaa lagu alxami karaa iyadoo la adeegsanayo hababka alxamida TIG, MIG, iyo iska caabbinta. Si kastaba ha ahaatee, alxamidu waxay u baahan tahay xakameyn taxaddar leh oo ku saabsan gelinta kulaylka iyo xulashada birta buuxinta si looga fogaado dildilaaca kulul. Daadinta xalka alxamida ka dib iyo gabowga ayaa laga yaabaa in loo baahdo si loo soo celiyo sifooyinka farsamada.

S: Waa maxay u dhigmayaasha Shiinaha ee Inconel 660?

A: U dhiganta Shiinaha ee Inconel 660 waa GH2132 (高温合金) loogu talagalay codsiyada hawada sare iyo heerkulka sare, iyo u dhiganta Jabbaan waa SUH660.

S: Foomamka badeecadaha noocee ah ayaa laga heli karaa Inconel 660?

A: Womic Steel waxay ku siisaa Inconel 660 tuubo aan kala go 'lahayn, tuubo la alxamayn, bir bir ah, saxan bir ah, gariirad bir ah, xariijin, flanges, qalab, foornooyin, silig, qalab xidhitaan, iyo waalka. Tilmaamaha badeecada oo dhammaystiran iyo cabbirka kala duwan ayaa lagu taxay qaybta helitaanka badeecada.

S: Inconel 660 ma u baahan yahay daaweyn kuleyl?

J: Haa. Inconel 660 waxay u baahan tahay in la nuugo xalka (980-1010°C) oo ay ku xigto gabow (675-705°C muddo 12-16 saacadood ah) si loo gaaro sifooyin farsamo oo ugu wanaagsan. Daawaynta gabowga waxay soo saartaa marxaladda γ' si loo xoojiyo.

La xiriir Womic Steel

Mareegta: www.womicsteel.com
Iimayl: sales@womicsteel.com

Taleefan / WhatsApp / WeChat:

Victor: +86 15575100681

Jack: +86 18390957568

Womic Steel – Lamaanahaaga lagu kalsoonaan karo ee Inconel 660 / Fasalka 660 (UNS S66286, SUH660, GH2132) tuubo aan kala go 'lahayn, bir bir ah, saxan bir ah, gariirad bir ah, flanges, qalab, foornooyin, iyo qalab loogu talagalay hawada sare, marawaxadaha gaaska, korontada, iyo codsiyada bolting heerkulka sare leh ee adduunka oo dhan. Raad-raac buuxa, shahaadada bulshada kala-soocidda, iyo dukumeentiyada EN 10204 Nooca 3.1/3.2 ayaa la heli karaa.